Sign In | Join Free | My xpshou.com
China SAMTION INTERNATIONAL LIMITED logo
SAMTION INTERNATIONAL LIMITED
SAMTION INTERNATIONAL LIMITED Focus on the export and production support of engineering plastics and special modified materials
Site Member

4 Years

Home > Plastic Resin Pellets Bulk >

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant

SAMTION INTERNATIONAL LIMITED
Contact Now

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant

  • 1
  • 2
  • 3

Brand Name : S-Plastic Verton

Model Number : AF3009

Certification : Datasheet,MSDS,ROHS,SGS,REACH,FDA,EU,UL,COC/COA ,please contact us

Place of Origin : ——

MOQ : 100KG

Price : *USD

Payment Terms : L/C, T/T, Western Union, MoneyGram

Supply Ability : To be negotiated

Delivery Time : To be negotiated

Packaging Details : 25KG/bag

Melt Volume Rate, MVR at 260°C/2.16 kg : ???

UL Recognized, 94V-0 Flame Class Rating (3) : 1.5

Contact Now

S-Plastics Verton AF3009 resin is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added
features of this material include: Antistat, Flame Retardant.


Property

TYPICAL PROPERTIES (1)
MECHANICAL Value Unit Standard
Tensile Stress, yield 42 MPa ASTM D 638
Tensile Stress, break 42 MPa ASTM D 638
Tensile Stress, yld, Type I, 5 mm/min 43 MPa ASTM D 638
Tensile Stress, brk, Type I, 5 mm/min 42 MPa ASTM D 638
Tensile Strain, yield 1.8 % ASTM D 638
Tensile Strain, break 1.9 % ASTM D 638
Tensile Strain, yld, Type I, 5 mm/min 1.8 % ASTM D 638
Tensile Strain, brk, Type I, 5 mm/min 2 % ASTM D 638
Tensile Modulus, 50 mm/min 4130 MPa ASTM D 638
Flexural Stress 55 MPa ASTM D 790
Flexural Stress, brk, 1.3 mm/min, 50 mm span 59 MPa ASTM D 790
Flexural Modulus 3440 MPa ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span 3450 MPa ASTM D 790
Tensile Stress, yield 43 MPa ISO 527
Tensile Stress, break 42 MPa ISO 527
Tensile Stress, yield, 5 mm/min 43 MPa ISO 527
Tensile Stress, break, 5 mm/min 42 MPa ISO 527
Tensile Strain, yield 1.8 % ISO 527
Tensile Strain, break 1.8 % ISO 527
Tensile Strain, yield, 5 mm/min 1.8 % ISO 527
Tensile Strain, break, 5 mm/min 1.9 % ISO 527
Tensile Modulus, 1 mm/min 3620 MPa ISO 527
Flexural Stress 61 MPa ISO 178
Flexural Stress, yield, 2 mm/min 61 MPa ISO 178
Flexural Modulus 3200 MPa ISO 178
Flexural Modulus, 2 mm/min 3200 MPa ISO 178
IMPACT Value Unit Standard
Izod Impact, unnotched, 23°C 224 J/m ASTM D 4812
Izod Impact, notched, 23°C 32 J/m ASTM D 256
Instrumented Impact Energy @ peak, 23°C 4 J ASTM D 3763
Multiaxial Impact 1 J ISO 6603
Izod Impact, unnotched 80*10*4 +23°C 15 kJ/m² ISO 180/1U
Izod Impact, notched 80*10*4 +23°C 3 kJ/m² ISO 180/1A
THERMAL Value Unit Standard
HDT, 0.45 MPa, 3.2 mm, unannealed 96 °C ASTM D 648
HDT, 1.82 MPa, 3.2mm, unannealed 87 °C ASTM D 648
CTE, -40°C to 40°C, flow 9.36E-05 1/°C ASTM E 831
CTE, -40°C to 40°C, xflow 6.12E-05 1/°C ASTM E 831
CTE, -40°C to 40°C, flow 9.4E-05 1/°C ISO 11359-2
CTE, -40°C to 40°C, xflow 6.2E-05 1/°C ISO 11359-2
CTE, 23°C to 60°C, flow 9.4E-05 1/°C ISO 11359-2
CTE, 23°C to 60°C, xflow 6.2E-05 1/°C ISO 11359-2
HDT/Bf, 0.45 MPa Flatw 80*10*4 sp=64mm 98 °C ISO 75/Bf
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm 90 °C ISO 75/Af
PHYSICAL Value Unit Standard
Density 1.31 g/cm³ ASTM D 792
Moisture Absorption, 50% RH, 24 hrs 2 % ASTM D 570
Mold Shrinkage, flow, 24 hrs 0.8 - 1 % ASTM D 955
Mold Shrinkage, xflow, 24 hrs 0.9 - 1.1 % ASTM D 955
Mold Shrinkage, flow, 24 hrs 0.93 % ISO 294
Mold Shrinkage, xflow, 24 hrs 1 % ISO 294
Density 1.31 g/cm³ ISO 1183
ELECTRICAL Value Unit Standard
Surface Resistivity 1.E+01 - 1.E+03 Ohm ASTM D 257
FLAME CHARACTERISTICS Value Unit Standard
UL Compliant, 94V-0 Flame Class Rating (3)(4) 1.5 mm UL 94 by GE
UL Recognized, 94V-0 Flame Class Rating (3) 1.5 mm UL 94
Source GMD, last updated:09/24/2008

Processing

Parameter
Injection Molding Value Unit
Drying Temperature 70 - 80 °C
Drying Time 4 hrs
Maximum Moisture Content 0.05 - 0.1 %
Melt Temperature 200 - 210 °C
Front - Zone 3 Temperature 205 - 215 °C
Middle - Zone 2 Temperature 195 - 205 °C
Rear - Zone 1 Temperature 180 - 195 °C
Mold Temperature 10 - 50 °C
Back Pressure 0.2 - 0.3 MPa
Screw Speed 30 - 60 rpm
Source GMD, last updated:09/24/2008

Other related products we recommend:

For more information please download the datasheet

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant S-Plastics Verton AF3009.pdf

Get The Latest Quotation

First-level distribution source in South China

Reduce procurement costs, improve supply stability,

Help you find the most suitable engineering plastic materials

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame RetardantClick to consult and get the latest quotation within 24 hours!

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant


China S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant wholesale

S-Plastic Verton AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: SAMTION INTERNATIONAL LIMITED
*Subject:
*Message:
Characters Remaining: (0/3000)